Investigating the relationship between mechanical properties and residual stress in the laser cladding process of Inconel 625 superalloy

AuthorsMohammad Reza Borhani, Mohammad Rajabi, Reza Shoja Razavi, Roohollah Jamaati
JournalHeliyon
Published At۲۰۲۳

Abstract