Experimental and Simulation-Based Investigations on the As-cast Microstructure of Inconel 657 Superalloy Produced by Investment Casting

AuthorsMasoud EsmaeilZadeh, Majid Abbasi
JournalMetallography Microstructure and Analysis
Published At۲۰۲۳

Abstract